MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV X5780B Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 5700B Series are highly engineered extrusion-grade thermoplastic vulcanizates with outstanding UV stability designed for demanding automotive interior and exterior sealing applications, including glass run channels, waistbelts, weather strips, seals and other profiles. This product is a medium hardness, medium density, high performance grade with low fogging and excellent color retention and elastic properties.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: UV Stabilizer

Features: Chemical Resistant; Good Processability; Medium Hardness; High Heat Resistance; Low Compression Set; Medium Density; Resilient; UV Resistant

Uses: Automotive Applications; Belts/Belt Repair; Profiles; Rubber Replacement; Seals; Weatherstripping

UL 94: UL 94

RoHS Compliance: RoHS Compliant

Automotive Specifications: DAIMLER MSAR 23 Type D; DAIMLER MSAR 23 Type E; GM GMP.E/P.037

UL File Number: QMFZ2.E54709

Form: Pellets

Processing Method: Injection Molding; Blow Molding; Extrusion; Profile Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³ISO 1183
Viscosity 330 cP
@Shear Rate 206 1/s,
Temperature 200 °C
330 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  80
@Time 5.00 sec
80
@Time 0.00139 hour
Extruded; ISO 868
 82
@Time 5.00 sec
82
@Time 0.00139 hour
Injection Molded; ISO 868
Tensile Strength at Break 9.03 MPa1310 psiFlow; ISO 37
 10.0 MPa1450 psiAcross Flow; ISO 37
 8.80 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
1280 psi
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 9.00 MPa
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
1310 psi
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  4.50 MPa
@Strain 100 %
653 psi
@Strain 100 %
Across Flow; ISO 37
 6.80 MPa
@Strain 100 %
986 psi
@Strain 100 %
Flow; ISO 37
 4.82 MPa
@Strain 100 %,
Treatment Temp. 150 °C
699 psi
@Strain 100 %,
Treatment Temp. 302 °F
Across Flow, Change in Air at 168 hr; ISO 188
 4.95 MPa
@Strain 100 %,
Treatment Temp. 135 °C
718 psi
@Strain 100 %,
Treatment Temp. 275 °F
Across Flow, Change in Air at 1000 hr; ISO 188
Elongation at Break 360 %360 %Flow; ISO 37
 590 %590 %Across Flow; ISO 37
 69.6 %
@Treatment Temp. 150 °C,
Time 605000 sec
69.6 %
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air at 168 hr; ISO 188
 478 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
478 %
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air at 168 hr; ISO 188
Tear Strength 47.3 kN/m270 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set  28 %
@Temperature 22.8 °C,
Time 79200 sec
28 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 41 %
@Temperature 70.0 °C,
Time 79200 sec
41 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 60 %
@Temperature 125 °C,
Time 252000 sec
60 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
Black
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 221 °C360 - 430 °FInjection, Melt
Rear Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Middle Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Front Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Nozzle Temperature 188 - 221 °C370 - 430 °FInjection
Zone 1 182 - 204 °C360 - 400 °FExtrusion
Zone 2 182 - 204 °C360 - 400 °FExtrusion
Zone 3 188 - 210 °C370 - 410 °FExtrusion
Zone 4 188 - 210 °C370 - 410 °FExtrusion
Zone 5 193 - 216 °C380 - 420 °FExtrusion
Die Temperature 193 - 216 °C380 - 420 °FExtrusion
Melt Temperature 193 - 216 °C380 - 420 °FExtrusion
Mold Temperature 10.0 - 65.6 °C50.0 - 150 °FInjection
Drying Temperature 82.2 °C180 °F
Dry Time 3.00 hour3.00 hour
Screw Speed 100 - 200 rpm100 - 200 rpmInjection
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1212 / 237703

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.