MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Ecoterra® HVI-E Hydraulic Oil ISO Grade 46
Categories: Fluid; Lubricant

Material Notes: Ecoterra HVI-E Hydraulic Oil is a high-quality, high viscosity index, zinc-free antiwear hydraulic oil developed for use in mobile equipment operating over a wide temperature range and in wet environments. It is specially formulated to emulsify readily with water to maintain effective lubrication in the presence of water. It is particularly recommended for use in off-road equipment manufactured by Hitachi, John Deere and others, operating under conditions where an emulsifiable hydraulic oil is specified or preferred. Ecoterra HVI-E Hydraulic Oil is formulated with an ashless (zinc-free) antiwear additive package to provide excellent wear protection for hydraulic pumps and motors, and to protect hydraulic system components against rust and corrosion. It has excellent oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life. It has a high viscosity index and low pour point for use over a wider temperature range than conventional antiwear hydraulic oils. It also has excellent low-temperature properties for cold start-ups. It will emulsify readily with water, and is resistant to excessive foam buildup that can cause poor or sluggish hydraulic system response. Ecoterra HVI-E Hydraulic Oil meets the performance requirements of all major hydraulic pump manufacturers, and is recommended for use in all types of high-pressure, high-speed hydraulic pumps. It also meets the performance requirements of Hitachi Advanced Hydraulic Oil where an emulsifiable hydraulic oil is recommended, and is fully compatible with the Hitachi fluid and with Hitachi seals and hoses.

Applications:

  • Hitachi excavators with 4,000-hour service intervals
  • Off-road mobile construction and forestry equipment, such as backhoes, bulldozers, crawlers, excavators, skid-steer loaders and motor graders, where the manufacturer recommends an emulsifiable ashless, zinc-free hydraulic oil
Ecoterra HVI-E Hydraulic Oil meets the requirements (except demulsibility) of the following industry and OEM specifications:
  • Bosch Rexroth RE 90220, Type HVLP
  • DIN 51524 Part 3, Antiwear Hydraulic Oils, Type HVLP
  • Eaton-Vickers M-2950-S, I-286-S
  • German Steel Industry SEB 181222
  • Hitachi Advanced Hydraulic Oil
  • ISO 11158:1997, Family H (Hydraulic Systems), Type HV
  • Parker Hannifin (Denison) HF-0, HF-1, HF-2
  • U.S. Steel 127
Features/Benefits:
  • Zinc-free formulation
  • High VI to reduce internal oil leakage and increase hydraulic system efficiency by up to 6% compared to conventional single-grade hydraulic oils
  • Excellent wear protection for hydraulic pumps and motors
  • Excellent oxidation resistance and thermal stability
  • Protects against rust and corrosion
  • Emulsifies readily with water
  • Good filterability
  • Good foam resistance
  • Suitable for year-round use

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.867 g/cc
Density 7.22 lb/gal
Viscosity Measurement 161Index
Saybolt Viscosity at 100°F 234 SUS
Saybolt Viscosity at 210°F 54.4 SUS
Kinematic Viscosity at 40°C (104°F) 46 cSt
Kinematic Viscosity at 100°C (212°F) 8.4 cSt
Oxidative Stability >= 8.33 hourRPVOT; ASTM D2272
ASTM Color 0.50ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.32[mg KOH/g]; ASTM D974
 
Thermal PropertiesOriginal ValueComments
Pour Point -48.0 °C
Flash Point 224 °CCOC
 
Descriptive Properties
Copper Corrosion1bASTM D130
Demulsibility80 ml30 mins @ 54°C, ASTM D1401
FZG Scuffing Test12 Failure Load StageASTM D5182

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik GETREN® P 3000 Emulsion
AISI 1040 Steel, oil quenched from 855°C (1570°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round

WCON5052 / 198305

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.