MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Outokumpu 4439 Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes:

Applications: Wet corrosion resistance and general service.

Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), and cold rolled strip/sheet forms.

Key Words: EN 1.4439; ASTM 317LMN
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³RT
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 640 MPa92800 psiOutokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Tensile Strength, Yield  270 MPa
@Strain 0.2 %
39200 psi
@Strain 0.2 %
EN min., RT; EN 10002-1
 310 MPa
@Strain 0.2 %
45000 psi
@Strain 0.2 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 350 MPa
@Strain 1 %
50800 psi
@Strain 1 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 150 MPa
@Strain 0.2 %,
Temperature 400 °C
21800 psi
@Strain 0.2 %,
Temperature 752 °F
EN min.; EN 10002-5
 185 MPa
@Strain 0.2 %,
Temperature 200 °C
26800 psi
@Strain 0.2 %,
Temperature 392 °F
EN min.; EN 10002-5
 225 MPa
@Strain 0.2 %,
Temperature 100 °C
32600 psi
@Strain 0.2 %,
Temperature 212 °F
EN min.; EN 10002-5
Elongation at Break 50 %50 %Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Modulus of Elasticity 200 GPa29000 ksiRT
 172 GPa
@Temperature 400 °C
24900 ksi
@Temperature 752 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000850 ohm-cm0.0000850 ohm-cmRT
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.0 µm/m-°C
@Temperature 100 °C
8.89 µin/in-°F
@Temperature 212 °F
 17.5 µm/m-°C
@Temperature 400 °C
9.72 µin/in-°F
@Temperature 752 °F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°FRT
Thermal Conductivity 14.0 W/m-K97.2 BTU-in/hr-ft²-°FRT
 20.0 W/m-K
@Temperature 400 °C
139 BTU-in/hr-ft²-°F
@Temperature 752 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.020 %0.020 %
Chromium, Cr 17.8 %17.8 %
Iron, Fe 65.24 %65.24 %
Molybdenum, Mo 4.1 %4.1 %
Nickel, Ni 12.7 %12.7 %
Nitrogen, N 0.14 %0.14 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Industeel CLC 18.15.4L 3% Mo Minimum Austenitic Stainless Steel
Carlson 317L Austenitic Stainless Steel
Crucible Steel SUE52 Martensitic Steel
Outokumpu 4438 High Performance Austenitic Stainless Steel
Sandvik 303-6RA11 Billet

NOUTOK30 / 18745

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.