MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Henkel Loctite® 3335 Epoxy Light Cure Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes:
Epoxy Light Cure AdhesivesLoctite® 3335 Epoxy Light Cure Adhesive
A one-part, medium viscosity, cationic epoxy. Excellent for surface cure - no oxygen inhibition. Low outgassing, very good high temperature resistance. Rigid, low shrinkage. Key Substrates: Metal, glass, thermoplastic Cure Type: Ultraviolet, Cationic Bonding Type: Epoxy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 6000 cP
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82
Elongation at Break 2.0 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 325 °F
Minimum Service Temperature, Air -65.0 °F
 
Descriptive Properties
ColorClear/Colorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® Durabond® E-00CL Epoxy Adhesive
Henkel Loctite® Tak Pak® 382 Instant Adhesive
Henkel Loctite® Durabond® M-21HP Epoxy Adhesive
Henkel Loctite® Durabond® E-214HP Epoxy Adhesive
Henkel Loctite® 4205 Thermally Resistant Ethyl Cyanoacrylate Bonding Adhesive

PLOCT085 / 51821

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.