MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Mobility and Materials MULTIFLEX™ G60 A 21 BT Z3519N0104A Thermoplastic Elastomer based Styrenic
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes:

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183
Spiral Flow 69.0 cm
@Pressure 8.00 MPa
27.2 in
@Pressure 1160 psi
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 6.90 MPa1000 psitype 1 v=500mm/min; ISO 37
Elongation at Break >= 300 %>= 300 %type 1 v=500mm/min, Cross direction; ISO 37
Tear Strength 27.0 kN/m154 pliparallel; ISO 34-1
Compression Set 12 %
@Temperature 23.0 °C
12 %
@Temperature 73.4 °F
ISO 815
 26 %
@Temperature 70.0 °C,
Time 86400 sec
26 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
 40 %
@Temperature 100 °C,
Time 86400 sec
40 %
@Temperature 212 °F,
Time 24.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 °C374 °FOptimum, Extrusion
 180 - 200 °C356 - 392 °FRange, Extrusion
Mold Temperature 10.0 - 60.0 °C50.0 - 140 °FInjection
 40.0 °C104 °FOptimum, Injection
Back Pressure 1.00 MPa145 psiInjection
 
Descriptive Properties
CompatibilityPolyolefins
Hold pressureas low as possibleInjection
Max. regrind level (%)10Injection
PolymerTPS
Regional AvailabilityEurope
 Near East/Africa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX4553 / 280499

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.