MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Copper Alloy, UNS C19005, TM04 Temper, Sheet & Strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Mill-hardened Temper, TM - Hard

Fabrication Properties: Good Suitability – Soldering, Brazing, Oxyacetylene Welding, Gas Shielded Arc Welding, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Fair Suitability – Coated Metal Arc Welding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.91 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 150 - 180
@Load 3.00 kg
150 - 180
@Load 6.62 lb
Tensile Strength 552 MPa80000 psiTypical
 517 - 593 MPa75000 - 86000 psi
Tensile Strength, Yield >= 441 MPa>= 64000 psi0.2% Offset
Elongation at Break >= 9.0 %>= 9.0 %
Tensile Modulus 130 GPa18900 ksi
Modulus of Rigidity 48.62 GPa7052 ksiCalculated
Poissons Ratio 0.340.34
Machinability 30 %30 %
Forgeability 50 %50 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000290 ohm-cm0.00000290 ohm-cm60% IACS
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 20.5 W/m-K142 BTU-in/hr-ft²-°F
Melting Point 1056 - 1079 °C1933 - 1974 °F
Solidus 1056 °C1933 °F
Liquidus 1079 °C1974 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 96.2 - 98.2 %96.2 - 98.2 %As Balance
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.050 %<= 0.050 %
Magnesium, Mg <= 0.010 %<= 0.010 %
Nickel, Ni 1.4 - 1.7 %1.4 - 1.7 %
Phosphorus, P <= 0.050 %<= 0.050 %
Silicon, Si 0.20 - 0.35 %0.20 - 0.35 %
Silver, Ag <= 0.50 %<= 0.50 %
Tin, Sn 0.020 - 0.30 %0.020 - 0.30 %
Zinc, Zn 0.20 - 0.70 %0.20 - 0.70 %
Zirconium, Zr <= 0.080 %<= 0.080 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC19005x2 / 291686

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.