MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teknor Apex Monprene® OM-10268 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene OM-10268 is a specialty thermoplastic elastomer, available in NAT, BLK and colors, designed for overmolding and co-extrusion applications like grips and anti-skid parts for consumer and industrial products. Monprene OM-10268 a medium hardness, low density, opaque grade that exhibits excellent adhesion to PC, ABS, and PC/ABS.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Abrasion Resistant; Bondability; Chemical Resistant; Good Adhesion; Good Processability; Light Stabilized; Medium Density; Medium Hardness; Medium Flow; Slip; Sunlight Resistant; Weather Resistant; Without Fillers

Uses: Appliances; Bonding; Cell Phones; Flexible Grips; Handles; Knobs; Overmolding; Power/Other Tools; Rubber Replacement; Soft Touch Applications; Sporting Goods; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion; Multi Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ASTM D792
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
10 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
 68
@Time 5.00 sec
68
@Time 0.00139 hour
ASTM D2240
Tensile Strength at Break 4.67 MPa678 psiDie C, 20 in/min, Across Flow; ASTM D412
 6.16 MPa894 psiDie C, 20 in/min, Flow; ASTM D412
Tensile Stress at Strain  2.25 MPa
@Strain 100 %
327 psi
@Strain 100 %
Die C, 20 in/min, Across Flow; ASTM D412
 2.78 MPa
@Strain 100 %
403 psi
@Strain 100 %
Die C, 20 in/min, Flow; ASTM D412
 3.73 MPa
@Strain 300 %
541 psi
@Strain 300 %
Die C, 20 in/min, Across Flow; ASTM D412
 4.22 MPa
@Strain 300 %
612 psi
@Strain 300 %
Die C, 20 in/min, Flow; ASTM D412
Elongation at Break 520 %520 %Die C, 20 in/min, Flow; ASTM D412
 570 %570 %Die C, 20 in/min, Across Flow; ASTM D412
Tear Strength 30.5 kN/m174 pliDie C, 20 in/min, Across Flow; ASTM D624
 30.5 kN/m174 pliDie C, 20 in/min, Flow; ASTM D624
Compression Set  17 %
@Temperature 22.8 °C,
Time 79200 sec
17 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 38 %
@Temperature 70.0 °C,
Time 79200 sec
38 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 50.0 °C122 °FUL 746
UL RTI, Mechanical with Impact 50.0 °C122 °FUL 746
UL RTI, Mechanical without Impact 50.0 °C122 °FUL 746
Flammability, UL94 HB
@Thickness 1.02 - 1.27 mm
HB
@Thickness 0.0400 - 0.0500 in
All Colors
 
Processing PropertiesMetricEnglishComments
Processing Temperature 166 - 221 °C330 - 430 °FMelt, Injection
Rear Barrel Temperature 138 - 188 °C280 - 370 °FInjection
Middle Barrel Temperature 154 - 199 °C310 - 390 °FInjection
Front Barrel Temperature 154 - 216 °C310 - 420 °FInjection
Nozzle Temperature 154 - 221 °C310 - 430 °FInjection
Zone 1 138 - 149 °C280 - 300 °F
Zone 2 149 - 160 °C300 - 320 °F
Zone 3 160 - 182 °C320 - 360 °F
Zone 4 160 - 182 °C320 - 360 °F
Die Temperature 160 - 182 °C320 - 360 °F
Mold Temperature 10.0 - 32.2 °C50.0 - 90.0 °FInjection
Drying Temperature 60.0 °C140 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Injection Pressure 1.38 - 5.52 MPa200 - 800 psiInjection
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Colors Available
 Grey
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0900 / 237391

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.