MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Pebax® MV 1041 SA 01 Polyether Block Amide (PEBA)
Categories: Polymer; Thermoplastic; Polyether Block Amide (PEBA)

Material Notes: Polyether block amide PEBAX® MV 1041 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on to a substrate offers excellent permeability to moisture vapor while remaining waterproof and offering an excellent barrier layer to bacteria. This SA grade is specially designed to medical and food uses.

Information provided by Arkema Group. Property data for dry samples, unless noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Water Absorption 12 %Sim. to ISO 62
Moisture Absorption 1.00 %Sim. to ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60
@Time 15.0 sec
ISO 868
Tensile Strength, Yield 15.0 MPaConditioned; ISO 527-1/-2
 17.0 MPaISO 527-1/-2
Film Elongation at Break, MD 500 %ISO 527-3
Film Elongation at Break, TD 600 %ISO 527-3
Elongation at Break >= 50 %Nominal, Conditioned; ISO 527-1/-2
 >= 50 %Nominal; ISO 527-1/-2
Elongation at Yield 26 %ISO 527-1/-2
 28 %Conditioned; ISO 527-1/-2
Tensile Modulus 253 MPaISO 527-1/-2
 270 MPaConditioned; ISO 527-1/-2
Flexural Modulus 270 MPaConditioned 15 days at 23°C - 50% RH; ISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 NB
@Temperature 23.0 °C
ISO 179/1eA
Film Tensile Strength at Break, MD 53.0 psiISO 527-3
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.50e+10 ohm-cmIEC 60093
Surface Resistance 5.00e+11 ohmIEC 60093
Dielectric Constant 5.0
@Frequency 1e+6 Hz
IEC 60250
 13
@Frequency 100 Hz
IEC 60250
Dielectric Strength 43.5 kV/mmIEC 60243-1
Dissipation Factor 0.0957
@Frequency 1e+6 Hz
IEC 60250
 0.626
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
Melting Point 170 °C10°C/min; ISO 11357-1/-3
Oxygen Index 23 %ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CInjection Molding; ISO 294
Mold Temperature 30.0 °CInjection Molding; ISO 10724
Injection Velocity 200 mm/secInjection Molding; ISO 294
Hold Pressure 30.0 MPaInjection Molding; ISO 294
 
Descriptive Properties
FeaturesAnti-static
 Heat stabilized or stable to heat
 Increased electrical conductivity
 Light stabilized or stable to light
 UV stabilized or stable to weather
FormPellets
Processing MethodsCasting
 Film Extrusion
 Injection Molding
 Other Extrusion
 Profile Extrusion
 Thermoforming
 Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Pebax® MV 1074 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 7233 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 5533 SP 01 Polyether Block Amide (PEBA)
Arkema Pebax® MV 1074 SP 01 Polyether Block Amide (PEBA)
Arkema Pebax® MH 2030 Polyether Block Amide (PEBA)

PZARKG729 / 142524

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.