The MC series is a material solution for applications requiring basic medical approvals such as ISO 10993-5 and food regulations. The compounds are available in translucent colors and can be colored in many different ways. They are produced exclusively on a special medical unit. Processing Method: Injection Molding, Extrusion Color / RAL DESIGN: Typical applications: - Pharmaceutical packaging
- Seals
- Valves
- Flexible Connections
Material advantages:- Adhesion to PP, PE
- Optimized compression set
- Free from animal ingredients
- Sterilizable (autoclave 134°C, ß-/y-radiation 2x35 kGy, EtO)
- KRAIBURG TPE Medical Service Package
Information provided by Kraiburg TPE |