MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Semicosil® 912 Silicone Gel
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: SEMICOSIL® 912 is a pourable, addition-curing, 2-part silicone rubber that cures to a soft silicone gel when mixed with ELASTOSIL® CAT PT, ELASTOSIL® CAT PT-F or ELASTOSIL® CAT UV.Special features:
  • two-part, 10 : 1 mixing ratio
  • low viscosity
  • modular system allows flexible adjustment of pot life and curing time by selection among different catalysts (no lot binding between base and catalyst)
  • fast curing at room temperature with Catalyst PT-F
  • long pot life at room temperature with Catalyst PT
  • extremely fast curing with Catalyst UV
  • low hardness
  • excellent tackiness
Application: Encapsulation of electronic components for the automotive and power electronics industries.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccLiquid
 0.970 g/cccured 30min at 150°C; ISO 2781
Viscosity 1000 cPdynamic; DIN EN ISO 3219
 1000 cPMix; ISO 3219
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %cured 30min at 150°C. "Transparent" but manufacturer does not quantify.
 90 %Transparent but manufacturer does not quantify.
 
Processing PropertiesOriginal ValueComments
Pot Life 5.00 minELASTOSIL® CAT PT-F
 120 minELASTOSIL® CAT PT
 >= 4320 minELASTOSIL® CAT UV
Gel Time 15.0 minELASTOSIL® CAT PT-F
 240 minELASTOSIL® CAT PT
 
Descriptive Properties
Colorclearcured 30min at 150°C
 clearliquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9414 / 204943

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.