MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV 24550D Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink 24550D is a high performance thermoplastic vulcanizate used in a variety of consumer and industrial applications. This product is available in NAT and BLK, is a high hardness, low density, UV stabilized grade designed for injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: General Purpose; Low Density; Low Flow; Low Specific Gravity; Slip; High Hardness; UV Stabilized

Uses: Gaskets; General Purpose; Glazing: Grommets; Plugs; Shock Absorbing Pads; Tubing

RoHS Compliance: RoHS Compliant

UL File Number: QMFZ2.E54709

Form: Pellets

Processing Method: Injection Molding; Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.932 g/cc0.0337 lb/in³ASTM D792
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  50
@Time 5.00 sec
50
@Time 0.00139 hour
Injection Molded; ASTM D2240
 52
@Time 1.00 sec
52
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 17.2 MPa2500 psiASTM D412
Elongation at Break 400 %400 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Processing Temperature 204 - 243 °C400 - 470 °FInjection, Melt
Rear Barrel Temperature 204 - 243 °C400 - 470 °FInjection
Middle Barrel Temperature 204 - 243 °C400 - 470 °FInjection
Front Barrel Temperature 204 - 243 °C400 - 470 °FInjection
Nozzle Temperature 204 - 243 °C400 - 470 °FInjection
Zone 1 193 - 232 °C380 - 450 °FExtrusion
Zone 2 193 - 232 °C380 - 450 °FExtrusion
Zone 3 193 - 232 °C380 - 450 °FExtrusion
Zone 4 193 - 232 °C380 - 450 °FExtrusion
Zone 5 193 - 232 °C380 - 450 °FExtrusion
Die Temperature 193 - 232 °C380 - 450 °FExtrusion
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °FInjection
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 120 rpm50 - 120 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Natural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1190 / 237681

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.