MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Haysite H1000 Polyester Laminate
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: Haysite Grade 1000 laminate sheet is an outstanding material that is used in applications requiring exceptional weather and corrosion resistance. Grade H1000's unique polyester resin system provides corrosion resistance in sunlight and harsh weather environments in addition to meeting NEMA GPO-3 specifications for track resistance, flame retardance, heat resistance and physical properties. H1000 is particularly qualified for applications in the transportation industry due to its' low smoke generation, low smoke toxicity & halogen-free flame retardants. H1000 meets the rigid New York City Transit - Specification #64. Transit Authorities use Grade H1000 under their 3rd rail ties to provide electrical insulation, corrosion protection, UV resistance & most importantly to insure low smoke/flame toxicity in case of electrical failure. H1000, in a pultruded profile shape is used for electrical insulation for electrical cables, conduit & 3rd rail protection for workers.

Information provided by Haysite

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.16 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 13000 psiCW; ASTM D638
 13500 psiLW; ASTM D638
Tensile Modulus 1.65e+6 psiLW; ASTM D638
 1.65e+6 psiCW; ASTM D638
Flexural Strength 22500 psiCW; ASTM D790
 25800 psiLW; ASTM D790
Flexural Modulus 1.33e+6 psiCW; ASTM D790
 1.88e+6 psiLW; ASTM D790
Compressive Strength 30000 psiFlatwise; ASTM D695
Izod Impact, Notched 10.4 ft-lb/inCW; ASTM D257
 12.0 ft-lb/inLW; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 290 V/milPerpendicular; ASTM D149
Arc Resistance 193 secASTM D495
Track Resistance >= 11 sec
@Thickness 6.35 mm
ASTM D2303
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.00 µin/in-°FASTM D696
Flammability, UL94 V-0
Flame Spread Index 20ASTM E84
Smoke Density 4.0 min6.3 Optical Density; ASTM E661
 
Descriptive Properties
Flame Resistance35 secondsBurning Time, ASTM D229
 80 secondsIgnition Time, ASTM D229
Radiant Panel15.9ASTM E162
Smoke and Toxicity DataAldehydes10 ppm, BSS7239
 Carbon Dioxide2400 ppm, BSS7239
 Carbon Monoxide700 ppm, BSS7239
 Hydrogen Bromide0.5 ppm, BSS7239
 Oxides of Nitrogen4.5 ppm, BSS7239
 Smoke Developed Index165, ASTM E84

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Haysite 46000 Polyester SMC, 30% Glass Reinforced
IDI Composites Rosite® C200BS ESD SMC, Conductive Thermoset Polyester, 10% Glass Reinforced
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP

PHAY517 / 142473

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.