MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Resinlab® AR 4305 White Metal Bonding Methacrylate Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Resinlab™ AR 4305 White is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 White forms tough, durable bonds to most plastics, composites, metals, ceramics, and woods in all combinations. Surface cleaning or preparation, or the use of primers, or chemical wipes is not required in almost all cases. AR 4305 White is a fast curing product with gelling of the mixed adhesive within 6-8 minutes and fixture in 10- 15 minutes at room temperature. The cure time was designed for high speed manufacturing processes where fast fixturing is required. AR 4305 White is easily dispensed from packaged cartridges or with commercial dispensing equipment as a non-sag, creamy gel, with no stringing. The product was designed to be used with static mixer tubes and has a balanced viscosity between parts. There are no abrasive fillers or extenders to reduce performance or cause wear in dispensing equipment.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 250000 cP250000 cPPart A, Spindle TD, 2.5 rpm; Uncured
 250000 cP250000 cPPart B, Spindle TD, 2.5 rpm; Uncured
 250000 cP250000 cPSpindle TD, 2.5 rpm; Curing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565Cured
Elongation at Yield 40 %40 %Cured
Adhesive Bond Strength 24.1 MPa3500 psialum/aluminum
 27.6 MPa4000 psisteel/steel
Impact >= 21>= 21[KJ/m^2]; FRP/FRP; auto side impact
Peel Strength >= 3.51 kN/m>= 20.0 plisteel/steel
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °FCured
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Flash Point 10.6 °C51.0 °FLCC; Uncured
 
Descriptive Properties
ColorNaturalPart A; Uncured
 WhitePart B; Uncured
Fixture Time (minutes)10-15Curing
Mix Ratio1:1Weight and Volume; Uncured
Working Time (minutes)6-8Curing

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRESL004 / 101418

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.