MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Mobil Turbo 319A-2
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Mobil Turbo 319A-2 is a fully synthetic lubricant developed to meet the performance requirements of Russian gas turbine aircraft engines which operate on mineral-oil-based lubricants. Formulated from a synthetic hydrocarbon combination of polyalphaolefin (PAO) and hindered ester based stock, Mobil Turbo 319A-2 is fortified with a unique chemical additive system. The resulting product has far superior thermal and oxidation stability than mineral-oil-based lubricants. The ability of Mobil Turbo 319A-2 to resist deterioration and deposit formation allows the potential for extended oil drain intervals and less frequent maintenance. The closely controlled viscosity of Mobil Turbo 319A-2 at -51º C, along with a -60ºC pour point, ensure good low-temperature fluidity, permitting engine starting and lubrication at low temperatures. Mobil Turbo 319A-2 exhibits excellent bulk oil stability at temperatures up to 200º C (392º F). The evaporation rate of Mobil Turbo 319A-2 at high temperatures is significantly lower than mineral-oil-based products, and helps minimize oil consumption. The lubricant has excellent resistance to foaming. Mobil Turbo 319A-2 is compatible with existing seal materials, including F Rubber (Viton A), H Rubber (Buna N), and silicone, as well as 11 metals used in gas turbine construction.

Mobil Turbo 319A-2 is recommended for aircraft gas turbine engines that normally operate on mineral-oil-based lubricants, as well as engines approved to operate on oils meeting the specifications listed below. Mobil Turbo 319A-2 is approved against the following specification of the Russian Central Institute of Aeronatutical Motors (CIAM): IMP-10; MS, 8P, MS-8RK; 36/1 Ku-A; VNII NP 50-1-4f and -4u; B3V and LZ-240; Mobil Turbo 319A-2 also meets U.S. Military Specification MIL-L-6081C, as well as the essential performance requirements of U.S. MIL-L-7808K, Grade 3.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.852 g/cc0.852 g/cc
Viscosity Measure  2917 cSt
@Temperature -40.0 °C
2917 cSt
@Temperature -40.0 °F
Kinematic Viscosity
 12545 cSt
@Temperature -51.0 °C
12545 cSt
@Temperature -59.8 °F
Kinematic Viscosity
Kinematic Viscosity at 40°C (104°F) 16.2 cSt16.2 cSt
Kinematic Viscosity at 100°C (212°F) 3.7 cSt3.7 cSt
Evaporation Loss 2.4 %2.4 %5 hr @ 175°C
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.0300.030
 
Thermal PropertiesMetricEnglishComments
Pour Point -60.0 °C-76.0 °F
Flash Point 234 °C453 °F
 
Descriptive Properties
Foam Sequence I, ASTM D113530/0
Foam Stability, after 1 min settling, mL0
Rubber Swell, %11.9H Rubber, 168 hr @ 70°C
 3F Rubber, 72 hr @ 175°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WEXXON347 / 75772

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.