MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SYNTHOS Krasten® 152 General Purpose Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Improved heat resistance, very good rheological properties.

Examples of Application:
Injection moulding – vegetable boxes for refrigerators, shower enclosure panels, CD and DVD cases. Blends with thermoplastic rubber.
Extrusion – thermoformed packaging – blends with high impact polystyrene, SBS.

Synthos was formerly known as Kaucuk. All information provided by Synthos.

Key Words: GPPS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inInternal; 50x50mm
Melt Flow 2.5 - 3.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.5 - 3.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Granulate; ISO 1133/H
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 150 MPa21800 psiH 358/30; Ø 50x4mm; ISO 2039-1
Tensile Strength at Break 50.0 MPa7250 psi5mm/min; ISO 527-2/1A/5
Elongation at Break 2.0 %2.0 %50mm/min; ISO 527-2/1A/5
Tensile Modulus 3.20 GPa464 ksi1mm/min; ISO 527-2/1A/1
Flexural Strength 80.0 MPa11600 psi2mm/min; 80x10x4mm; ISO 178
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
80x10x4mm; ISO 180/1U
Charpy Impact Unnotched  1.60 J/cm²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
80x10x4mm; ISO 179/1eU
 2.60 J/cm²
@Temperature 23.0 °C
12.4 ft-lb/in²
@Temperature 73.4 °F
80x10x4mm; ISO 179/1fU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cm500V; Ø 93x3mm; IEC 93
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm500V; Ø 93x3mm; IEC 93
Dielectric Constant <= 2.7
@Frequency 50 Hz
<= 2.7
@Frequency 50 Hz
500V; Ø 93x3mm; IEC 250
Dielectric Strength >= 60.0 kV/mm>= 1520 kV/inTransformer Oil; Ø 93x3mm; IEC 243-1
Dissipation Factor <= 0.0020
@Frequency 50 Hz
<= 0.0020
@Frequency 50 Hz
500V; Ø 93x3mm; IEC 250
Comparative Tracking Index >= 250 V>= 250 VSolution A; Ø 93x3mm; IEC 112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °F80x10x4mm; ISO 75-2/Af
Vicat Softening Point 91.0 °C196 °F50°C/h; 50N; 10x10x4mm; ISO 306/B50
 95.0 °C203 °F50°C/h; 10N; 10x10x4mm; ISO 306/A50
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Tested in EZÚ Praha
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Tested in EZÚ Praha
Glow Wire Test 650 °C1200 °FØ 93x3mm; IEC 695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Axion Polymers Axpoly® PS01 3000 General Purpose Polystyrene
Axion Polymers Axpoly® PS01 3009 Green General Purpose Polystyrene
Ineos Nova 2110 General Purpose Crystal Polystyrene
Axion Polymers Axplas® PS07 0000 General Purpose Polystyrene
American Polymers API 645-21 Polystyrene

PSYNT018 / 82631

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.