MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay IGEPAL® CO 710 Surfactant
Categories: Fluid

Material Notes: Chemical Name: NONYLPHENOXY POLY(ETHYLENEOXY)ETHANOL, BRANCHED

CAS: 68412-54-4

Available in: Asia Pacific, Europe, Latin America and North America

Applications: IGEPAL© CO-710 is an excellent primary nonionic surfactant, recommended especially for the emulsion polymerization of acrylic, vinyl acrylic, styrene butadiene and styrene acrylic polymers. Such polymers find application in latex paints, adhesives, paper coatings and textile applications. IGEPAL© CO-710 is one of a series of Rhodia ethoxylated alkylphenol nonionic surfactants with different HLBs. Since differences in HLB affect emulsification and stabilization properties, the Igepal series allows the user to select the surfactant that will provide effective particle size control, low levels of coagulum, latex stability and trouble-free commercial production.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/cc
Solids Content 99.5 %Oven
 100 %
pH 6.0 - 8.010% Solution
Viscosity 210 - 350 cP
Surface Tension 34 dynes/cmat CMC
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.50 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClear to Slightly Hazy Viscous LiquidRP-0064
Cloud point70-74°C1% Solution, RP-0124
Color<100APHA, RP-0134
Critical Micelle Concentration (%)0.05
HLB number13.6
Hydroxyl Number50-54 mg KOH/gRP-0245
Ionic ChargeNonionic
Moles of Ethylene Oxide10-11
Neutralization Number<0.5 mg KOH/gpH7, RP-0343

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay ANTAROX® BL 225 E Surfactant
Solvay IGEPAL® CO 970 Surfactant
Solvay IGEPAL® CO 880 Surfactant
Solvay IGEPAL® CO 730 Surfactant
Solvay IGEPAL® CO 720 Surfactant

WRHOD149 / 137380

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.