MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ PC 6900 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: EMERGE™ PC 6900 is a specially designed ignition-resistant polycarbonate alloy. It combines high flow, high heat and high strength together. It is especially suited for thin-wall applications and has excellent high gloss aesthetics. EMERGE™ PC 6900 has a UL 94 V-0 rating at 1.0 mm. This material does not contain chlorine or bromine additives.

Main Characteristics:

  • Ignition resistant
  • High flow
  • High gloss
Applications:
  • Thin-Wall Powder Device Housings
  • Consumer Electronics
  • Information technology equipment
  • Computer housings

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 in/inASTM D955
Melt Flow 18 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 123
@Thickness 3.20 mm
Injection molded; ASTM D785
Tensile Strength, Yield 65.0 MPa
@Thickness 3.20 mm
Injection Molded; ASTM D638
Elongation at Break 70 %
@Thickness 3.20 mm
Injection Molded; ASTM D638
Flexural Strength 96.5 MPa
@Thickness 3.20 mm
Injection Molded; ASTM D790
Flexural Modulus 2650 MPaInjection Molded; ASTM D790
Izod Impact, Notched 150 J/m
@Thickness 3.20 mm
Injection Molded; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 66.0 µm/m-°CASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
@Thickness 3.20 mm
Unannealed, Injection Molded; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °CUnannealed, Injection Molded; ASTM D648
Vicat Softening Point 116 °CASTM D1525
Flammability, UL94 V-2
@Thickness 0.500 mm
 V-1
@Thickness 0.800 mm
 V-0
@Thickness 1.00 mm
 5VB
@Thickness 2.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 221 - 260 °C
Mold Temperature 71.0 - 102 °C
Drying Temperature 91.0 - 102 °C
Dry Time 3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo EMERGE™ PC 8130-10 Polycarbonate Resin
Trinseo CALIBRE™ 301-15 Polycarbonate Resin
Trinseo CALIBRE™ MEGARAD™ 2081-15 Polycarbonate Resin
Trinseo EMERGE™ 8702 Polycarbonate
Trinseo EMERGE™ PC 8130-15 Polycarbonate Resin

PTRINS9043 / 197543

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.