MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Sarlink® TPE ME-2255D BLK 111 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ME-2255D BLK 111 is a general purpose thermoplastic elastomer used in automotive applications, including exterior. Sarlink ME-2255D BLK 111 is a high hardness, low density, RoHS compliant grade suitable for injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Abrasion Resistant; Good Color Stability; Good Flow; Good Melt Strength; Good Moldability; Good Processability; Good Processing Stability; High Hardness; Low Density; Low Fogging; Low Specific Gravity; Without Fillers

Uses: Automotive Applications; Automotive Exterior Parts

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.962 g/cc0.0348 lb/in³ASTM D792
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
 5757ASTM D2240
Tensile Strength at Break 17.6 MPa2550 psiASTM D412
Elongation at Break 600 %600 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 227 - 249 °C440 - 480 °F
Middle Barrel Temperature 227 - 249 °C440 - 480 °F
Front Barrel Temperature 227 - 249 °C440 - 480 °F
Nozzle Temperature 227 - 249 °C440 - 480 °F
Melt Temperature 227 - 249 °C440 - 480 °F
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1062 / 237553

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.