MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Covestro MONDUR® 1515 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Mondur 1515 is a polymeric diphenylmethane diisocyanate (PMDI) prepolymer.

Properties / Applications: Mondur 1515 polyisocyanate is used in the production of rigid polyurethane foams, especially for the appliance industry. As with any product, use of Mondur 1515 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.236 g/cc
@Temperature 32.2 °C
 1.24 g/cc
@Temperature 25.0 °C
 1.244 g/cc
@Temperature 15.6 °C
Viscosity 235 - 435 cP
 200 cP
@Temperature 35.0 °C
 400 cP
@Temperature 23.9 °C
 1000 cP
@Temperature 12.8 °C
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 200 °CPMCC
 
Descriptive Properties
Acidity0.01-0.03%
AppearanceDark brown liquid
Content29.8-31.2%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0897 / 202680

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.