MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group TuffGel 338 High Strength Silicone Gel
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: TufGel 338 is a clear, tough, moderately cross-linked silicone elastomer, which has good room temperature cure adhesion to many substrates. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provide excellent moisture protection.

Key Features:

  • One to one mix ratio
  • High strength
  • Long gel time
  • Dispensing equipment not necessary
  • Good adhesion to many substrates including glass, aluminum and copper

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/ccUncatalyzed, TufGel 338A
 0.970 g/ccUncatalyzed, TufGel 338B
Viscosity 350 cPUncatalyzed, TufGel 338B
 500 cPUncatalyzed, TufGel 338A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 35
@Temperature 25.0 °C,
Time 173000 sec
 45
@Treatment Temp. 150 °C,
Time 1800 sec
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
@Temperature 150 °C
 60.0 min
@Temperature 100 °C
Gel Time 480 minCatalyzed
 
Descriptive Properties
AppearanceTransparentUncatalyzed, TufGel 338A
 TransparentUncatalyzed, TufGel 338B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Northstar Polymers MPP-F07A Easy Hand-Mixable/Pourable Flexible Foam
NuSil Lightspan™ LS-3246 Silicone Optical Gel
Eurofoam Porocell POR 304 B-OPC EPDM Foam
Dow 3-6651 THERMALLY CONDUCTIVE ELASTOMER, KIT
CHT Group TuffGel 339 High Strength Silicone Gel

PACC2133 / 199521

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.