MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Domo TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: This grade has good mechanical properties, flame retardant rating UL94 V0 and glow-wire at 960°C. It is specially suitable for pieces such as: switches, timers, etc. This product is available in Natural.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.62 g/cc0.0585 lb/in³ISO 1183/A
Water Absorption 0.95 %
@Temperature 23.0 °C,
Time 86400 sec
0.95 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0075 cm/cm0.0075 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 114 MPa16500 psiISO 527 Type 1A
Elongation at Break 1.8 %1.8 %ISO 527 Type 1A
Tensile Modulus 11.4 GPa1650 ksiISO 527 Type 1A
Charpy Impact Unnotched 3.70 J/cm²17.6 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 41.0 kV/mm1040 kV/inIEC 60243
Dissipation Factor 0.0150.015IEC 60250
Comparative Tracking Index 450 V450 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 197 °C387 °FISO 75/Af
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
1210
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
1210
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
1210
Glow Wire Ignition Temperature  825 °C
@Thickness 0.800 mm
1520 °F
@Thickness 0.0315 in
ISO 60695-2-13
 850 °C
@Thickness 1.60 mm
1560 °F
@Thickness 0.0630 in
ISO 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
ISO 60695-2-12
 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 230 - 235 °C446 - 455 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone235-240°C
Mixing Zone240-245°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, Conditioned
Domo TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, Conditioned
Domo TECHNYL® 1021GF6 PA6, 30% glass fiber, DRY
Domo TECHNYL® 1011R PA6, DRY
Domo TECHNYL® C 218 V 30 PA6, 30% glass fiber, Conditioned

PRHOD783 / 138014

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.