HIFOR Xtreme® SC74877 is an enhanced clarity hexene LLDPE designed for blown film extrusion applications requiring high strength and clarity. This material is highly stabilized, and contains medium anti-block and process aid. This product has some 21 CFR clearances. Application/Uses: Blown film extrusion, Heavy Duty Films.Information provided by Westlake Chemical Corporation. |