MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akro-Plastic Akromid® C3 GF 30 1 black (4363) PA 6.6/6 Dry, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: Description: AKROMID C3 GF 30 1 black (4363) is a 30% glass fiber reinforced, heat stabilized polyamide 6.6/6 – Blend. Applications are mainly components in mechanical engineering and the automotive industry where good flowability is required.

Additive: Heat Stabilizer

Features:

  • Good Flow
  • Heat Stability
Uses:
  • Automotive Applications
  • Engineering Parts

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183
Filler Content 30 %ISO 1172
Moisture Absorption 1.9 %
@Temperature 70.0 °C
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cmISO 294-4
Melt Flow 45 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
Spiral Flow 92.0 cmCross section: 7 mm x 3.5 mm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 185 MPa5 [mm/min]; ISO 527-2
Elongation at Break 3.0 %5 [mm/min]; ISO 527-2
Tensile Modulus 9300 MPa1 [mm/min]; ISO 527-2
Flexural Strength 275 MPa2 [mm/min]; ISO 178
Flexural Modulus 9200 MPa2 [mm/min]; ISO 178
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 75.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CDIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 257 °CUnannealed; ISO 75/B
Deflection Temperature at 1.8 MPa (264 psi) 247 °CUnannealed; ISO 75/A
Deflection Temperature at 8.0 MPa 204 °CUnannealed; ISO 75/C
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Feed Temperature 60.0 - 80.0 °C
Nozzle Temperature 280 - 295 °C
Zone 1 225 - 300 °C
Zone 2 225 - 300 °C
Zone 3 225 - 300 °C
Zone 4 225 - 300 °C
Melt Temperature 280 - 310 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 °C
Dry Time 2.00 hour
Hold Pressure 30.0 - 80.0 MPa
Back Pressure 5.00 - 10.0 MPa
 
Descriptive Properties
Resistance to AcetaldehydeFail40% Conc. at 23°C
Resistance to Acetic AcidPass20% Conc. at 23°C
Resistance to AcetonePass100% Conc. at 23°C
Resistance to AcetonitrilePass100% Conc. at 23°C
Resistance to AcrylonitrilePass100% Conc. at 23°C
Resistance to Allyl alcoholFail96% Conc. at 23°C
Resistance to Amyl alcoholPass100% Conc. at 23°C
Resistance to Aqueous AmmoniaPass10% Conc. at 23°C
Resistance to BenzeneFail100% Conc. at 40°C
Resistance to BiodieselPass100% Conc. at 23°C
Resistance to Boric acidFail100% Conc. at 23°C
Resistance to Brake fluid (DOT 4)Fail100% Conc. at 130°C
Resistance to Calcium chloride, alcoholicFail10% Conc. at 23°C
Resistance to Calcium chloride, aqueousPass10% Conc. at 23°C
Resistance to Carbonic acidPass100% Conc. at 60°C
Resistance to Caustic potash solution, aqueousPass50% Conc. at 23°C
Resistance to ChlorineFail100% Conc. at 23°C
Resistance to Chlorine waterFail100% Conc. at 23°C
Resistance to Chloroacetic acidFail50% Conc. at 23°C
Resistance to Chromic acidFail10% Conc. at 23°C
Resistance to CyclohexanePass100% Conc. at 23°C
Resistance to CyclohexanolPass100% Conc. at 23°C
Resistance to Dichloro-Acetic acidFail50% Conc. at 23°C
Resistance to Diesel fuel (DIN 51601)Pass100% Conc. at 23°C
Resistance to EthanolPass96% Conc. at 23°C
Resistance to Ethylene glycol/waterFail50% Conc. at 120°C
Resistance to Formaldehyde, aqueousPass10% Conc. at 23°C
Resistance to Formic acidFail2% Conc. at 23°C
Resistance to GlycerinPass100% Conc. at 23°C
Resistance to Hydraulic oil H and HL (DIN 51524)Pass100% Conc. at 100°C
Resistance to Hydrogen chloride, gasFail100% Conc. at 23°C
Resistance to Iso-octanolPass100% Conc. at 23°C
Resistance to IsopropanolPass100% Conc. at 23°C
Resistance to MethanolPass100% Conc. at 23°C
Resistance to Methylene chlorideFail100% Conc. at 23°C
Resistance to Motor oil (SAE 10W-40)Pass100% Conc. at 130°C
Resistance to Natural GasPass100% Conc. at 23°C
Resistance to Nitric acidFail40% Conc. at 23°C
Resistance to Oleic acidPass100% Conc. at 23°C
Resistance to OzoneFail100% Conc. at 23°C
Resistance to PhenolFail100% Conc. at 23°C
Resistance to Phosphoric acidFail30% Conc. at 23°C
Resistance to Potassium chloride, aqueousPass10% Conc. at 23°C
Resistance to Potassium permanganate, aqueousFail10% Conc. at 23°C
Resistance to Sodium chloride, aqueousPass10% Conc. at 23°C
Resistance to Sodium hydroxide solution, aqueousPass1% Conc. at 23°C
Resistance to Sodium hypochlorite, aqueousFail10% Conc. at 23°C
Resistance to Transmission oil (ATF m 1375.4)Pass100% Conc. at 150°C
Resistance to Urea, aqueousPass20% Conc. at 23°C
Resistant to Carbon disulfidePass100% Conc. at 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® C3 GF 30 5 XTC (4499) PA66/6 Dry, 30% Glass Filled
BASF Ultramid® B3ZG6 BK30564 30% Glass Filled PA6 (Dry)
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Dry)
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Conditioned)
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Dry)

PAKRO350 / 182937

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.