MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Total LLDPE LL 1810 Linear Low Density Polyethylene - Blown Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: LL 1810 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.

LL 1810 can be processed at high output rates with moderate extrusion pressure, good bubble stability and gauge control on blown film machine designed for LLDPE.

LL 1810 can advantageously be blended with LDPE or other PE resins used in blown film mono extrusion or coextrusion to improve film properties.

LL 1810 is suited for many applications in the field of consumer, industrial, food or hygiene packaging such as collation shrink, liners, Form-Fill-Seal, heavy-duty sacks, refuse sacks or other bags and non-packaging applications like agriculture films e.g. tunnel and mulching films.

Contains antioxidant.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.919 g/cc0.919 g/ccISO 1183
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.0 MPa1600 psiISO 527-3
Film Tensile Strength at Yield, TD 11.0 MPa1600 psiISO 527-3
Film Elongation at Break, MD 800 %800 %ISO 527-3
Film Elongation at Break, TD 850 %850 %ISO 527-3
Elmendorf Tear Strength, MD 7.10 g/micron180 g/milISO 6383-2
Elmendorf Tear Strength, TD 12.2 g/micron310 g/milISO 6383-2
Dart Drop Test 150 g0.331 lbISO 7765-1
Film Tensile Strength at Break, MD 38.0 MPa5510 psiISO 527-3
Film Tensile Strength at Break, TD 33.0 MPa4790 psiISO 527-3
1% Secant Modulus, MD 215 MPa31200 psiISO 178
1% Secant Modulus, TD 245 MPa35500 psiISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 122 °C252 °FISO 11357-3
Vicat Softening Point 100 °C212 °FISO 306
 
Optical PropertiesMetricEnglishComments
Haze 11 %11 %ISO 14782
Gloss 60 %60 %at 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 220 °C356 - 428 °FExtrusion Temp
Die Opening >= 0.180 cm>= 0.0709 in
Blow-up Ratio (BUR) 2.0 - 3.02.0 - 3.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Baystar™ Lumicene® mPE M 2710 EP Metallocene Medium Density Polyethylene Film Resin
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 50 Gauge
Dow ELITE™ 5401G Enhanced Polyethylene Resin
Dow ELITE™ 5400G Enhanced Polyethylene Resin
Dow ELITE™ 5100G Enhanced Polyethylene Resin

PTOTAL735 / 130460

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.