MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sumitomo Bakelite Plyophen 43204 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: DESCRIPTION: Plyophen 43204 is a liquid one-step resin in ethanol.

APPLICATION: Plyophen 43204 has been specifically designed for both high and low pressure laminating applications employing glass cloth and other reinforcing agents. Properly constructed laminates made with Plyophen 43204 display superior strength and modulus retention at operating temperatures up to 400°F. (Higher temperatures may be tolerated for short periods).

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccDCT 5075
pH 8.558.55DCT 4064A
Viscosity 475 cP
@Temperature 25.0 °C
475 cP
@Temperature 77.0 °F
DCT 4003F
 
Processing PropertiesMetricEnglishComments
Gel Time 950 min
@Temperature 135 °C
950 min
@Temperature 275 °F
Sunshine; DCT 5091
 
Descriptive Properties
Non Volatile (%)66.5DCT 4005A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSUMIT184 / 193989

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.