MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell CirculenRecover C14 EP448T Polypropylene, Impact Copolymer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: CirculenRenew C14 EP448T is part of the Circulen© product family of circular and sustainable solutions. CirculenRenew C14 polymer reduces the carbon footprint as it replaces fossil feedstock through using renewable raw materials made from bio-based waste and residue oils. The renewable content of CirculenRenew C14 is measured by an accredited third party laboratory and stated as a parameter on the Certificate of Analysis (CoA). CirculenRenew C14 EP448T is a drop-in solution and therefore doesn’t require any adaptation of the existing processing equipment. CirculenRenew C14 EP448T is a nucleated heterophasic copolymer with antistatic additivation used in injection molding applications. CirculenRenew C14 EP448T has a high flow, good impact/stiffness balance. CirculenRenew C14 EP448T is typically used by customers in opaque containers, housewares, toys and closures.

Status: Commercial - Active

Availability: Africa-Middle East; Europe

Application: Caps & Closures; Housewares; Opaque Containers; Sports, Leisure & Toys

Market: Consumer Products; Rigid Packaging

Processing Method: Injection Molding

Attribute: Contains Antistat; High Flow; Impact Copolymer; Medium Impact Resistance; Medium Stiffness; Nucleated

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 48.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
48.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 27.0 MPa3920 psiISO 527-1, -2
Elongation at Yield 5.00 %5.00 %ISO 527-1, -2
Tensile Modulus 1.25 GPa181 ksiISO 527-1, -2
Charpy Impact, Notched  0.250 J/cm²
@Temperature -20.0 °C
1.19 ft-lb/in²
@Temperature -4.00 °F
Type 1, Edgewise, Notch A; ISO 179
 0.350 J/cm²
@Temperature 0.000 °C
1.67 ft-lb/in²
@Temperature 32.0 °F
Type 1, Edgewise, Notch A; ISO 179
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FUnannealed; ISO 75B-1, -2
Vicat Softening Point 151 °C304 °FA50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9075 / 324010

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.