MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials MEGUM™ 16510 Adhesive
Categories: Polymer; Thermoset

Material Notes: Solvent-based 1-coat adhesive for the bonding of polar elastomers to metal or other rigid substrates during vulcanization.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.800 - 0.830 g/ccISO 845
 1.10 g/ccDry Film
Solids Content >= 1.0 %
Volatile Organic Compounds (VOC) Content 790 g/l
Viscosity 2.0 cP
Brookfield Viscosity >= 0.20 cP
 
Thermal PropertiesOriginal ValueComments
Flash Point 13.0 °CASTM D 92
 
Processing PropertiesOriginal ValueComments
Processing Temperature 120 °C
@Time 601 sec
Oven pre-bake
Dry Time 0.333 hourApplication technique
Shelf Life 9.00 Month
 
Descriptive Properties
ColorTransparent
CompatibilityFluoropolymers
Dilution, parts diluent0.5 - 2spraying
 1 - 5dipping
 undilutedbrushing
PolymerAdhesive
Recommended application film thickness1
SolventEthanol
Theoretical coverage (m²/L)45

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX4834a / 290946

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.