MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Epoxies, Etc 20-3068, Cat 190 Epoxy Adhesive and Potting Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 20-3068 is a room temperature curing, two component, epoxy potting compound and adhesive. This product provides good water resistance, adhesion, and toughness. The 20-3068 Epoxy System meets the Food and Drug Administration (FDA) regulations permitting use in “indirect” food contact applications. The raw materials used in the products comply with the FDA regulations of Title 21 Code of Federal Regulations under Sections 175.105 and 175.300.

Features:

  • Excellent adhesion
  • Excellent chemical and corrosion resistance
  • Excellent electrical insulation

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/cc
Viscosity 3500 cP3500 cPMixed
Storage Temperature 50.0 - 77.0 °C122 - 171 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888
Tensile Strength 73.1 MPa10600 psi
Elongation at Break 6.0 %6.0 %
Flexural Strength 117 MPa17000 psi
Compressive Strength 108 MPa15600 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  1.30e+13 ohm-cm
@Temperature 100 °C
1.30e+13 ohm-cm
@Temperature 212 °F
 >= 1.00e+16 ohm-cm
@Temperature 25.0 °C
>= 1.00e+16 ohm-cm
@Temperature 77.0 °F
 2.00e+16 ohm-cm
@Temperature 60.0 °C
2.00e+16 ohm-cm
@Temperature 140 °F
Dielectric Constant 3.47
@Frequency 1e+6 Hz
3.47
@Frequency 1e+6 Hz
Dissipation Factor 0.034
@Frequency 1e+6 Hz
0.034
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 62.0 µm/m-°C34.4 µin/in-°F
Glass Transition Temp, Tg 80.0 °C176 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 40.0 min
@Load 0.100 kg
40.0 min
@Load 0.221 lb
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorClear/Yellowish
Mix Ratio100:15By weight, Resin: Catalyst

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX033 / 316710

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.