MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro Platilon® H2 Thermoplastic Adhesive Film
Categories: Polymer; Adhesive; Film

Material Notes: Product Description: Platilon H is the trade name for thermoplastic adhesive films made by Epurex Films. The range currently includes films based on:
  • copolyamide
  • thermoplastic polyurethane
  • copolyester
Properties: Platilon® H films combine excellent adhesion properties and easy processability with outstanding mechanical and chemical properties:
  • good resistance to detergents
  • high resistance to greases, oils and fuels
Applications: The broad raw material range of Platilon® H allows excellent bonding to various substrates. Bonding applications include:
  • automotive industry: for example interior parts and sound protection
  • insulation industry
  • wallpaper industry
  • home textiles
  • non wovens and foams

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
 
Thermal PropertiesMetricEnglishComments
Softening Point >= 100 °C>= 212 °FTMA Onset
 110 - 120 °C230 - 248 °FKofler bench knife
 
Descriptive Properties
Appearancetransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Platilon® HU2 Thermoplastic Adhesive Film
Covestro Platilon® M2234 Polyether-Blockamide Film
Covestro Platilon® 2202 AC Polyurethane Film
Chevron Phillips 7105DKT LLDPE Blown Film Resin, Hexene Copolymer
Chevron Phillips 6109 LLDPE Blown Film Resin, Butene Copolymer

PCOVEST0960 / 202743

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.