MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Astralloy AstraWear 400F 400 BHN Wear Resistant Steel
Categories: Metal; Ferrous Metal; Martensitic

Material Notes: AstraWear 400F is a water tempered martensitic steel, with typical hardness of 400 BHN (42.5 HRC), which offers real response to wear from abrasion. Its resistance, high hardness, and high yield strength, make AstraWear 400F suitable for use in applications that require resistance to wear from scraping or moderate impact. AstraWear 400F offers a real benefit for the service life of equipment and allows for significant reduction of design thickness because its resistance to wear makes it up to 3 times more durable than A572-50 (S355) grade. AstraWear 400F welds easily and has excellent forming properties, which combine to facilitate processing. This steel is especially suited for applications in quarries, construction, mines, cement plants, and the iron and steel industry, among others.

Information provided by Astralloy, a Nucor Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 360 - 444360 - 444
Tensile Strength 1240 MPa180000 psi
Tensile Strength, Yield 1000 MPa145000 psi
Elongation at Break 16 %
@Thickness 50.8 mm
16 %
@Thickness 2.00 in
Charpy Impact  27.1 J
@Temperature -40.0 °C
20.0 ft-lb
@Temperature -40.0 °F
Transerse
 33.9 J
@Temperature -40.0 °C
25.0 ft-lb
@Temperature -40.0 °F
Longitudinal
Bend Radius, Minimum  3.0 t
@Diameter <=50.8 mm
3.0 t
@Diameter <=2.00 in
Perpendicular to Grain Direction
 4.0 t
@Diameter <=50.8 mm
4.0 t
@Diameter <=2.00 in
Parallel to Grain Direction
 
Component Elements PropertiesMetricEnglishComments
Boron, B <= 0.0030 %<= 0.0030 %
Carbon, C <= 0.16 %<= 0.16 %
Chromium, Cr <= 0.60 %<= 0.60 %
Iron, Fe >= 96 %>= 96 %As Balance
Manganese, Mn <= 1.55 %<= 1.55 %
Molybdenum, Mo <= 0.50 %<= 0.50 %
Nickel, Ni <= 0.80 %<= 0.80 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si <= 0.40 %<= 0.40 %
Sulfur, S <= 0.010 %<= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ovako S355JR EN10025-2:2004 Steel
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition CH 900
Astralloy AstraWear 500F 500 BHN Wear Resistant Steel
Sandvik Chromflex 12C27 Strip steel
ASTM A36 Steel, bar

NNUCOR914 / 233188

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.