MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Westlake EF1820 Low Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Westlake Polyethylene EF1820 is a low density polyethylene with outstanding optical properties, making this material an excellent choice for food packaging applications.

    Application/Uses
  • Bread bags
  • Food packaging
  • Retail bags

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Outstanding optical properties
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ASTM D1505
Thickness 38.1 microns1.50 mil
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 300 %300 %ASTM D882
Film Elongation at Break, TD 800 %800 %ASTM D882
Dart Drop 2.10 g/micron53.3 g/milASTM D1709
Dart Drop Test 80.0 g0.176 lbASTM D1709
Film Tensile Strength at Break, MD 33.8 MPa4900 psiASTM D882
Film Tensile Strength at Break, TD 22.8 MPa3300 psiASTM D882
1% Secant Modulus, MD 207 MPa30000 psiASTM D882
1% Secant Modulus, TD 241 MPa35000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 6.5 %6.5 %ASTM D1003
Gloss 60 %60 %at 45º; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 193 °C360 - 380 °Fwith BUR of 2.4:1 or higher
Blow-up Ratio (BUR) 2.42.4
 
Descriptive Properties
ProcessFilm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake EF1807 Low Density Polyethylene
LyondellBasell Plexar® PX1007 Extrudable Tie-Layer Resin - Anhydride Modified EVA

PWESF080 / 84517

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.