MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Total Lacqrene® 814(EU) High Impact Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: LACQRENE® 814 is a PBDE free high impact, flame retardant polystyrene with excellent UV stability, rated UL 94 V0 @ 2mm and UL 94 5 VA @ 3mm.

Application

Covers for electrical equipment, External covers for office equipment, TV back covers,

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Water Absorption <= 0.10 %<= 0.10 %ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/in
Melt Flow 6.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133H
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 19.0 MPa2760 psiISO 527-2
Tensile Strength, Yield 23.0 MPa3340 psiISO 572-2
Elongation at Break 45 %45 %ISO 527-2
Flexural Modulus 2.00 GPa290 ksiISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 88.0 °C190 °F50N (T° increase = 5°C/h); ISO 306B50
 97.0 °C207 °F10N (T° increase = 50°C/h); ISO 306A50
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 240 °C<= 464 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFINAA053 / 38489

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.