MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Saint-Gobain Norton® V740 Multipurpose Pressure Sensitive Adhesive Sealant Foam
Categories: Polymer; Adhesive; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: Description: Medium Density, Multipurpose Foam: Norseal V740 is a closed-cell polyvinyl chloride foam sealant with pressure-sensitive adhesive on one side designed to provide an economical solution to seal against light, air and moisture. Because Norseal has been specially formulated to provide superior performance with a reduced density foam, it is ideal for applications such as appliance seals, wall panels, die-cut gaskets, and window and door weatherstripping.

Conformable and Dimensionally Stable: Norseal provides excellent conformability to curved and irregular shapes, and is resistant to weather, fungi and oxidation, ensuring a long sealing life. In addition, Norseal is dimensionally stable. It will not drip, ooze or run when under compression. And, Norseal remains flexible at low temperatures.

Pressure Sensitive Adhesive: The pressure-sensitive adhesive on one side keeps the foam in place during many assembly operations. A paper liner eliminates stretching during installation, and the roll remains intact when handled. Norseal V740 series is available in gray and black.

Features/Benefits:
  • Multipurpose medium density foam offers an economical alternative to caulks and other sealants
  • Conforms to curved and irregular shapes
  • Resistant to weather, fungi and oxidation
  • Flexible at low temperatures
  • Dimensionally stable
Typical applications include: Appliance seals, electronic equipment, wall panels, die-cut gaskets, window and door weatherstripping, access doors, truck, cab and body seals, foundation to sill gaskets, and seals for flashing. All data based on a 0.25 inch test sample.(Available in thicknesses from 1/16" to 3/8".)
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.144 g/cc0.00520 lb/in³ASTM D1667
Water Absorption 2.5 %2.5 %% by volume; NTP-35
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 2828ASTM D2240
Tensile Strength, Yield 0.276 MPa40.0 psiASTM D-412 (Die A)
Elongation at Break 100 %100 %ASTM D-412 (Die A)
Compressive Modulus 0.0000138 GPa0.00200 ksiCompression Deflection, Compressed to 30%.; ASTM D1667
 0.0000241 GPa0.00350 ksiForce to Compress, Value for 30% compression.
Compression Set 8.0 %8.0 %Constant Deflection, Compressed to 30%.; Norton Test Procedure 37
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0403 W/m-K0.280 BTU-in/hr-ft²-°FASTM-C-518
Maximum Service Temperature, Air 71.1 °C160 °F
Minimum Service Temperature, Air -26.1 °C-15.0 °F
 
Descriptive Properties
ColorGray and Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Norton® V990 Poly Liner Pressure Sensitive Adhesive Foam Sealant
Saint-Gobain Norton® V980 Paper Liner Pressure Sensitive Adhesive Foam Sealant
Saint-Gobain Norton® V770 Low-Density Pressure Sensitive Adhesive Sealant Foam
Saint-Gobain Norton® V730 Pressure Sensitive Adhesive Sealant Foam
Parker Chomerics CHO-BOND® 320 Pressure Sensitive Adhesive

PSTGQZ483 / 68997

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.