MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Cabot ELFTEX® 415 Specialty Carbon Black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product highlights: ELFTEX 415 specialty carbon black is a low structure product designed to exhibit high color strength and gloss in lithographic gloss inks.

Key applications: ELFTEX 415 specialty carbon black is suitable for use in multiple applications including lithographic gloss ink and liquid inks.
Lithographic Inks: ELFTEX 415 specialty carbon black is a neutral tone carbon black with low vehicle demand and good color strength. It is used primarily in lithographic gloss ink applications where good color strength and high gloss are required. Because of its low vehicle demand, it is particularly well suited for applications where a highly loaded base is desired.
Liquid Inks: ELFTEX 415 specialty carbon black is also suitable for use in liquid inks requiring high gloss and low viscosity. The dispersibility of ELFTEX 415 specialty carbon black depends on the equipment used and the formulation. A product with similar morphology, ELFTEX 410 pigment black, is available in an easier to handle pelleted form.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Mesh Size 325 Mesh<25 ppm residue; ASTM D-1514
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 1.0 %ASTM D-1509
 
Descriptive Properties
Iodine absorption97 mg/gASTM D-1510
OAN54 cc/100gASTM D-2414
Tint1.24ASTM D-3265

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT122 / 315857

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.