MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Datenblatt Alsint Pure Grain™
Categories: Ceramic

Material Notes: Resulting from our purposeful selection of ultrapure initial raw materials and our deliberate engineered microstructure, parts manufactured from the newly developed aluminium oxide material provide: 1. high corrosion resistance to chemical attacks 2. high imperviousness in gaseous atmospheres 3. low creep tendency at high temperatures 4. high purity 5. high strength As per the characteristics specified above, components show a strikingly high durability in the large variety of applications for sheath tubes.

information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 3.90 g/cc>= 0.141 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 300 - 380 GPa43500 - 55100 ksi
Flexural Strength 350 MPa
@Temperature 20.0 °C
50800 psi
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 - 9.00 µm/m-°C
@Temperature 20.0 - 1000 °C
4.44 - 5.00 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 25.0 W/m-K
@Temperature 200 °C
174 BTU-in/hr-ft²-°F
@Temperature 392 °F
Maximum Service Temperature, Air 1800 °C3270 °Ffor load bearing elements
 
Component Elements PropertiesMetricEnglishComments
Al2O3 >= 99.8 %>= 99.8 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
316 Stainless Steel, spring tempered wire, 13 mm diam.
316 Stainless Steel, spring tempered wire, 1.6 mm diam.
316 Stainless Steel, soft tempered wire, 13 mm diam.
316 Stainless Steel, soft tempered wire, 1.6 mm diam.
316 Stainless Steel, annealed wire, 13 mm diam.

CMORF8056 / 203533

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.