Physical Properties | Metric | English | Comments |
---|
Density | 1.10 g/cc | 0.0397 lb/in³ |
Moisture Absorption | 2.1 % @Temperature 70.0 °C | 2.1 % @Temperature 158 °F |
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in |
Linear Mold Shrinkage, Transverse | 0.022 cm/cm | 0.022 in/in |
Spiral Flow | 0.800 cm | 0.315 in |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength, Yield | 63.0 MPa | 9140 psi |
Elongation at Break | >= 35 % | >= 35 % |
Tensile Modulus | 2.70 GPa | 392 ksi |
Flexural Strength | 90.0 MPa | 13100 psi |
Flexural Modulus | 2.50 GPa | 363 ksi |
Flexural Strain at Break | 7.5 % | 7.5 % |
Charpy Impact Unnotched | NB @Temperature 23.0 °C | NB @Temperature 73.4 °F |
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C | 4.76 ft-lb/in² @Temperature -22.0 °F |
| 1.50 J/cm² @Temperature 23.0 °C | 7.14 ft-lb/in² @Temperature 73.4 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm |
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm |
Comparative Tracking Index | 600 V | 600 V |
|
Thermal Properties | Metric | English | Comments |
---|
Melting Point | 262 °C | 504 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C | 158 °F |
Flammability, UL94 | HB @Thickness 1.60 mm | HB @Thickness 0.0630 in |
|
Processing Properties | Metric | English | Comments |
---|
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F |
Nozzle Temperature | 280 - 295 °C | 536 - 563 °F |
Zone 1 | 260 - 300 °C | 500 - 572 °F |
Zone 2 | 260 - 300 °C | 500 - 572 °F |
Zone 3 | 260 - 300 °C | 500 - 572 °F |
Zone 4 | 260 - 300 °C | 500 - 572 °F |
Melt Temperature | 280 - 310 °C | 536 - 590 °F |
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F |
Drying Temperature | 80.0 °C | 176 °F |
Dry Time | 2.00 hour | 2.00 hour |
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi |
Back Pressure | 5.00 - 10.0 MPa | 725 - 1450 psi |
|
Descriptive Properties |
---|
Resistance to Acetaldehyde | Fail |
Resistance to Acetic Acid | Pass |
Resistance to Acetone | Pass |
Resistance to Acetonitrile | Pass |
Resistance to Acrylonitrile | Pass |
Resistance to Allyl alcohol | Fail |
Resistance to Amyl alcohol | Pass |
Resistance to Aqueous Ammonia | Pass |
Resistance to Benzene | Fail |
Resistance to Biodiesel | Pass |
Resistance to Boric acid | Fail |
Resistance to Brake fluid (DOT 4) | Fail |
Resistance to Calcium chloride, alcoholic | Fail |
Resistance to Calcium chloride, aqueous | Pass |
Resistance to Carbonic acid | Pass |
Resistance to Caustic potash solution, aqueous | Pass |
Resistance to Chlorine | Fail |
Resistance to Chlorine water | Fail |
Resistance to Chloroacetic acid | Fail |
Resistance to Chromic acid | Fail |
Resistance to Cyclohexane | Pass |
Resistance to Cyclohexanol | Pass |
Resistance to Dichloro-Acetic acid | Fail |
Resistance to Diesel fuel (DIN 51601) | Pass |
Resistance to Ethanol | Pass |
Resistance to Ethylene glycol/water | Fail |
Resistance to Formaldehyde, aqueous | Pass |
Resistance to Formic acid | Fail |
Resistance to Glycerin | Pass |
Resistance to Hydraulic oil H and HL (DIN 51524) | Pass |
Resistance to Hydrogen chloride, gas | Fail |
Resistance to Iso-octanol | Pass |
Resistance to Isopropanol | Pass |
Resistance to Methanol | Pass |
Resistance to Methylene chloride | Fail |
Resistance to Motor oil (SAE 10W-40) | Pass |
Resistance to Natural Gas | Pass |
Resistance to Nitric acid | Fail |
Resistance to Oleic acid | Pass |
Resistance to Ozone | Fail |
Resistance to Phenol | Fail |
Resistance to Phosphoric acid | Fail |
Resistance to Potassium chloride, aqueous | Pass |
Resistance to Potassium permanganate, aqueous | Fail |
Resistance to Sodium chloride, aqueous | Pass |
Resistance to Sodium hydroxide solution, aqueous | Pass |
Resistance to Sodium hypochlorite, aqueous | Fail |
Resistance to Transmission oil (ATF m 1375.4) | Pass |
Resistance to Urea, aqueous | Pass |
Resistant to Carbon disulfide | Pass |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding