MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Go Yen Chemical GOYENCHEM-ADC-110 Blowing Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Characteristic:
  • Excellent foaming ability
  • The series products can be used in various application after special dispersal process.
  • It can be used in normal atmospheric pressure foaming and pressure foaming
  • Thin powder
  • It could get white plastic foam.
  • Great resiliency.
  • It gives end-products even and solid foaming structure.
Applications:
  • <> It mainly use in PVC.
  • polyethylene, polypropylene, polystyrene
  • polyamide, nylon-6, ABS resin
  • rubber system : chloroprene rubber, Acrylonitrile butadiene rubber, natural rubber, butyl rubber, styrene butadiene rubber, silicone rubber. Foaming processing of chloroprene rubber and various synthetic materials.
  • various thermosetting resin: PU, UP, acrylic
  • high blowing slice products
  • It’s suitable for producing high valued foaming synthetic leather
  • other special applications

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size <= 8.0 µm<= 8.0 µmfineness 96%
Ash 0.10 %0.10 %
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 200 - 210 °C392 - 410 °F
 
Descriptive Properties
Amount of Generating Gas205-215 ml/g
Appearancethin powder
Colorpale yellow
Heat loss0.0015

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN361 / 266669

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.