MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Scotchkote™ 162PWX Epoxy Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: 3M Scotchkote Epoxy Coating 162PWX is a 100% solid two-part epoxy coating that has been specifically developed for the long term protection of drinking water pipelines, storage and process tanks or vessels and related steelwork immersed or in contact with potable water. Scotchkote epoxy coating 162PWX is designed for high build single coat applications by either plural feed hot airless spray equipment, brush or roller.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³
Solids Content 100 %100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Water Absorption 1.05 %1.05 %21 days; ASTM D570
Thickness 508 microns20.0 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D2240
Tensile Strength at Break 23.5 MPa3410 psiASTM D638
Elongation at Break 1.4 - 2.0 %1.4 - 2.0 %ASTM D638
Flexural Strength 57.00 MPa8267 psiASTM D790
Impact Test 4.50 J3.32 ft-lbASTM G14 (modified)
Abrasion 113113[mg] CS-17, 1000 cycles; ASTM D4060
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 50.0 °C122 °F
 71.0 °C160 °Fonset
 
Processing PropertiesMetricEnglishComments
Cure Time 240 min4.00 hourTouch Dry
 360 min6.00 hourHard Dry, 1 hr when surface temp at 50°C
 10100 min168 hourFull Cure
 
Descriptive Properties
AppearanceGray or Blue
Pencil Hardness5HASTM D3363

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chesterton ARC S1HB Sprayable high-viscosity, 100% solids, advanced coating
Chesterton ARC 10 Paste grade machinable composite
3M Scotchkote™ HTX 517 Epoxy HT Lining
3M Scotchkote™ 162HB Epoxy Coating

PMM35340 / 170087

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.