MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dover Chemical DOVERSPERSE 3NR Water Dispersed Chlorinated Alkanes
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Doversperse 3-NR is an aqueous emulsion of liquid chlorinated paraffin of medium chain length. Because of its non-ionic base, it is useful in both anionic and cationic emulsion systems. In addition to contributing to flame retardancy, Doversperse 3-NR improves adhesion, imparts chemical and water resistance, and allows the user to formulate aqueous rather than solvent based systems. Application areas include adhesives, rubber coatings, inks, carpet backings, paper and fabric coatings.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc
@Temperature 25.0 °C
1.20 g/cc
@Temperature 77.0 °F
Brookfield Viscosity 220 cP
@Temperature 25.0 °C
220 cP
@Temperature 77.0 °F
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 36 %36 %
 
Descriptive Properties
AppearanceCream White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDOVER052 / 217671

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.