MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

HB Fuller 42327/52343 Polyurethane Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: 42327-52343 is a medium-hardness, semi-flexible two–component polyurethane adhesive designed for bonding applications requiring resilient bonds, non-sag application and enhanced adhesion to flexible substrates. 42327-52343 is suitable for bonding metals, ceramics, natural rubber, thermosetting polymers and select types of unprepared thermoplastic substrates such as ABS, Polycarbonate and Nylon.

Features and Benefits:

  • Excellent bond strength to a wide variety of substrates
  • Low Exotherm
  • Good thermal performance
  • Good chemical resistance
  • Non Sag
  • High Flexibility

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/cc
Viscosity 16000 cP16000 cPPart A
 83000 cP83000 cPPart B
Storage Temperature 16.0 - 27.0 °C60.8 - 80.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength 25.6 MPa3710 psi50% RH; ASTM D638
Elongation at Break 160 %160 %50% RH; ASTM D638
Shear Strength 4.40 MPa638 psiOverlap, ABS, IPA wipe; ASTM D1002
 7.20 MPa1040 psiOverlap, Nylon 6-6, abraded; ASTM D1002
 13.1 MPa1900 psiOverlap, Electrogalvanized Steel, IPA wipe; ASTM D1002
 13.8 MPa2000 psiOverlap, PC, IPA wipe; ASTM D1002
 14.3 MPa2070 psiOverlap, GFPC, abraded; ASTM D1002
 15.2 MPa2200 psiOverlap, Aluminum, abraded; ASTM D1002
 20.7 MPa3000 psiOverlap, Cold Rolled Steel, abraded; ASTM D1002
 22.3 MPa3230 psiOverlap, Stainless Steel, abraded; ASTM D1002
 24.9 MPa3610 psiOverlap, E-Coat Steel, IPA wipe; ASTM D1002
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min0.250 hourTack Free Time
 120 min
@Temperature <=80.0 °C
2.00 hour
@Temperature <=176 °F
Full Cure
 1080 min
@Temperature <=25.0 °C
18.0 hour
@Temperature <=77.0 °F
Full Cure
Gel Time 3.00 - 5.00 min
@Load 0.0100 kg
3.00 - 5.00 min
@Load 0.0221 lb
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorBlack
ConsistencyThixotropic Paste
Mix Ratio100:100Volume
 100:125Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL062 / 316853

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.