MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lion Stereon™ 721AC Styrene-butadiene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Stereon™721AC is a solution polymerized styrene-butadiene block copolymer that has been designed as an impact modifier for thermoplastic ABS resin. The low solution viscosity of this product makes it particularly attractive for high rubber loading systems. Stereon™721AC also contains a non-volatile antioxidant stabilizer system and has a very low gel content.

Information provided by Lion Elastomer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/cc
Volatiles <= 0.60 %<= 0.60 %ASTM D5668
Viscosity 28 - 36 cP28 - 36 cP5.43% in Toluene; ASTM D445
Mooney Viscosity 33 - 43
@Temperature 100 °C
33 - 43
@Temperature 212 °F
ML/4; ASTM D1646
Ash <= 0.20 %<= 0.20 %ASTM D5667
 
Chemical PropertiesMetricEnglishComments
Styrene Content 4.5 - 8.5 %4.5 - 8.5 %Block; ASTM D3314
 9.0 - 11.5 %9.0 - 11.5 %Bound; ASTM D5775
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -92.0 °C-134 °FASTM E1356
 
Descriptive Properties
Color0-10 APHAASTM D1209
Content<0.007%Toluene Insolubles
Dissolving Time<4 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLION081 / 317990

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.