VESTAMID® E62-S3 BK V303579 is a PA 12 elastomer consisting of PA 12 segments and softening segments. The material is free of volatile or migrating plasticizer. The VESTAMID® E represent thermoplastic elastomers generically characterized as polyether block copolyamides (PEBA) consisting of PA 12 and polyether segments. VESTAMID® E62-S3 BK V303579 is especially developed for sport shoe soles. It has good impact strength at low temperatures. VESTAMID® E62-S3 BK V303579 is supplied as cylindrical pellets in moisture-proof packaging, ready for processing. The process temperatures should be within a range of 190°C – 230°C. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C. Dry properties listed below Industrial Sector: Automotive and Mobility, Sustainable, Industry and Engineering, Sports and Lifestyle Sustainability: Sustainable electricity Delivery form: Pellets, Granules Optics: Translucent Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels Electrical: Insulating Conformity: Automotive Additives: Unfilled Special Characteristics: Light-stabilized, High heat resistant Color: Black Additives: Heat stabilizerInformation provided by Evonik. |