MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Morgan Advanced Ceramics Pythagoras Alumina Silicate
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Refactory materials, widely used in furnace construction and as furnace rollers. Sillimantin grades are porous; Pythagoras grades are dense

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.35 - 3.00 g/cc0.0849 - 0.108 lb/in³Fired
Porosity 0.00 - 11 %0.00 - 11 %Apparent, % water absorption
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 60.0 - 150 GPa
@Temperature 20.0 °C
8700 - 21800 ksi
@Temperature 68.0 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm
@Temperature 20.0 °C
1.00e+13 ohm-cm
@Temperature 68.0 °F
dense grades
Dielectric Strength 17.0 kV/mm
@Temperature 20.0 °C
432 kV/in
@Temperature 68.0 °F
dc, dense grades
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.70 - 6.30 µm/m-°C
@Temperature 20.0 - 1000 °C
3.17 - 3.50 µin/in-°F
@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.800 - 0.900 J/g-°C0.191 - 0.215 BTU/lb-°F
Thermal Conductivity 1.40 - 6.00 W/m-K
@Temperature 200 °C
9.72 - 41.6 BTU-in/hr-ft²-°F
@Temperature 392 °F
Maximum Service Temperature, Air 1250 - 1350 °C2280 - 2460 °Fworking

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Sillimantin 60 Alumina Silicate
Morgan Advanced Ceramics MF120F Alumina Silicate
Aremco AREMCOLOX™ 502-1400 (Bisque-fired) Machinable Alumina

CMORG44 / 90422

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.