MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Rogers Arlon 27122T125 Cured Silicone Rubber/Skive Tape Laminate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Design/Construction:
  • Side 1: Cured Silicone Rubber
  • Substrate: 5.0 mil Etched Skive Tape bonded to one side

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 127 microns5.00 milSkive Tape
 3050 microns120 milSide 1
 3180 microns125 milOverall Thickness
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040Silicone Property
Tensile Strength 6.21 - 7.58 MPa900 - 1100 psiSilicone Property
Elongation at Break 585 - 615 %585 - 615 %Silicone Property
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 4.44 °C
12.0 Month
@Temperature 40.0 °F
 
Descriptive Properties
ColorNatural
Total Product Weight (oz/yd2)143

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARL9714 / 148867

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.