MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Universal Wire Works 55 Nickel Alloy Welding Wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Universal nickel alloy 55 is designed to arc weld cast iron, malleable iron, ductile iron, and Ni-Resist as well as welding cast irons to steel and high nickel alloys. Alloy 55 is also used for welding high phosphorous irons and casting that have heavy for thick sections. Castings can be welded without preheat, however a more machinable deposit and less stresses will be built up in the welding zone if a preheat of 400 degrees is used. Alloy 55 can be used in all positions with either AC or DCRP.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Key Words: AWS A5.15 Class ENiFe-Cl
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.2 %1.2 %
Copper, Cu 0.10 %0.10 %
Iron, Fe 45 %45 %
Manganese, Mn 0.30 %0.30 %
Nickel, Ni 53 %53 %
Silicon, Si 0.70 %0.70 %
Sulfur, S 0.0050 %0.0050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Universal Wire Works 99 Nickel Alloy Welding Wire
CMSX-2 Nickel Alloy Composition Spec
Copper nickel 30%, UNS C71500
Haynes 230® alloy, GMAW deposit weld metal
Commercial Bronze, UNS C22000 (90-10 Bronze), H06 Temper wire

NUWW102 / 19637

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.