MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Rogers Arlon 15370P020 0.020" (0.508 mm) Uncured Silicone Rubber on a Mylar Carrier
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Design/Construction:
Interleave: Polyethylene
Side 1: Uncured Silicone Rubber
Carrier: Mylar

Appearance: Pink high viscosity gum

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccArlon SQA-TMS-024
Thickness 1.50 milCarrier
 3.00 milInterleave
 20.0 milOverall; Arlon SQA-TMS-003
 20.0 milSide 1; Arlon SQA-TMS-003
Deformation 0.060 %Silicone Property; Arlon SQA-TMS-005
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 21.1 °C
From date of manufacture
 
Descriptive Properties
ColorBlueInterleave
 Pink
Plasticity6 mmArlon SQA-TMS-005
Total Product Weight (oz/yd2)19Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® 814 Polyester Film, 48 Gauge
Armacell Monarch® F-05021 (Black) Neoprene, EPDM, SBR Blend Foam
DuPont Teijin Films Mylar® 823 Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® 840 Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® 850H Polyester Film, 48 Gauge

PARL112 / 125298

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.