MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical LUPOY SR3108L PC, High Impact  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Impact Modified

Material Notes: Description: Injection Molding, PC, High Flow, High Impact, White Color Only

Application: BLU Mold frame for Mobile Devices

CAS: 103598-77-2 and 13463-67-1

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/ccASTM D792
Maximum Moisture Content 0.020Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 25 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 117ASTM D785
Tensile Strength, Yield 550 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 100 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Flexural Yield Strength 900 kg(f)/cm²
@Thickness 3.20 mm
10mm/min; ASTM D790
Flexural Modulus 23000 kg(f)/cm²
@Thickness 3.20 mm
10mm/min; ASTM D790
Izod Impact, Notched >= 60.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 124 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
UL RTI, Electrical 80.0 °C
UL RTI, Mechanical with Impact 80.0 °C
UL RTI, Mechanical without Impact 80.0 °C
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 250 - 280 °CInjection Molding
Middle Barrel Temperature 260 - 290 °CInjection Molding
Front Barrel Temperature 260 - 290 °CInjection Molding
Nozzle Temperature 260 - 280 °CInjection Molding
Melt Temperature 260 - 280 °CInjection Molding
Mold Temperature 60.0 - 90.0 °CInjection Molding
Drying Temperature 100 - 120 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Back Pressure 0.981 - 3.92 MPaInjection Molding
Screw Speed 40 - 70 rpmInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eurotec® Tecotek® PC40 NL VB02 PC, unfilled, UV stabilized, high impact, natural
Eurotec® Tecotek® PC30 NL RX PC, unfilled, improved flow & low temperature impact, natural
A. Schulman Diamond ABS 9401 Injection Molding Grade, Ultra High Impact
LG Chemical LUPOY SC1004L PC, High Impact
TPI Porene® ABS-SP-100 Super High Impact ABS Resin

PLAY539 / 148549

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.