MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Aquivion® E87-03 Tetrafluoroethylene + SFVE (TFE+SFVE)  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Aquivion® PFSA ionomer membranes are melt-extruded products based on the unique Short Side Chain (SSC) copolymer of Tetrafluoroethylene and a Sulfonyl Fluoride Vinyl Ether (SFVE) F2C=CF-O-CF2CF2-SO2F of low molecular weight produced by Solvay Specialty Polymers. Aquivion® PFSA ionomer membranes are available in the acid form and feature lower Equivalent Weight (EW) than most competitive proton exchange membranes. The SSC copolymer allows higher crystallinity, improved mechanical properties and better proton conductivity. Typical applications of Aquivion® PFSA membranes are PEM fuel cells, water electrolyzers, H2 separators, pervaporation or gas humidification systems. Membrane grades are presently subdivided in two families E87 and E79 which exhibit different EW of 870 or 790 g/eq SO3H. The value is controlled systematically according to an internal titration procedure. Nominal thicknesses are 30 or 50 µm - with E87 also available at 100. Others may be available upon request. For some applications, it can be recommendable to use chemically stabilized membranes (recognizable through their S-suffix). E79 grades are exclusively available in their chemically stabilized form.

Additional Information: HEALTH, SAFETY AND ENVIRONMENT - Aquivion® PFSA membranes are not harmful if used and handled according to standard processing procedures (see for example the "Guide to the Safe Handling of Fluoropolymer Resins" issued by the Society of the Plastics Industry). If handled inappropriately, membranes may release harmful toxic chemicals. PACKAGING, SHIPMENT AND STORAGE - The membranes are usually available in sheets of customized formats or rolls in various lengths (dimensions are based on dry product conditioned at 23 °C and 50 % Relative Humidity). They are sealed in an inert environment with a multilayer protection film before packaging inside a shock-protected cardboard box. It is recommended to store the product in a clean, controlled humidity environment and protected from direct sun light or other sources of heat.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.06 g/ccextrapolated to 0 % water adsorption; ASTM D792
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD >= 11.0 MPa
@Temperature 23.0 °C
50 mm/min; 50% RH; ASTM D638
Film Tensile Strength at Yield, TD >= 11.0 MPa
@Temperature 23.0 °C
50 mm/min; 50% RH; ASTM D638
Film Elongation at Break, MD >= 140 %
@Temperature 23.0 °C
50 mm/min; 50% RH; ASTM D638
Film Elongation at Break, TD >= 180 %
@Temperature 23.0 °C
50 mm/min; 50% RH; ASTM D638
Film Elongation at Yield, MD >= 8.0 %
@Temperature 23.0 °C
50 mm/min; 50% RH; ASTM D638
Film Elongation at Yield, TD >= 8.0 %
@Temperature 23.0 °C
50 mm/min; 50% RH; ASTM D638
Film Tensile Strength at Break, MD >= 25.0 MPa
@Temperature 23.0 °C
50 mm/min; 50% RH; ASTM D638
Film Tensile Strength at Break, TD >= 20.0 MPa
@Temperature 23.0 °C
50 mm/min; 50% RH; ASTM D638
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
Equivalent Weight (EW)850 to 890 g/eqeq = mol SO3H
GenericTFE+SFVE
Membrane27.0 to 33.0 µmThickness
 55.0 to 69.0 g/m²Weight
Power Factor> 0.500 W/cm²
Total Acid Capacity> 1.20 meq/gInternal Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y7573 / 135636

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.