MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Covestro Arcol® PPG-1000 Polypropylene Glycol
Categories: Polymer; Thermoset

Material Notes: Characterization: Arcol PPG-1000 is a 1,000-molecular-weight polypropylene glycol.

Properties / Applications: Arcol PPG-1000 polyether polyol is a 1,000 molecular-weight polypropylene glycol. The terminal end-groups are predominantly secondary hydroxyls and have a relatively low reactivity. It is compatible with most polyether polyols and can be blended with other diols or triols to achieve desirable modifications of product properties. This polyol is acidified with a low level of phosphoric acid, making it suitable for use in isocyanate-terminated prepolymers. Arcol PPG-1000 polyol is used in a broad range of urethane foam and other applications including coatings, solvent and water-based adhesives, caulks, sealants, elastomers, defoamers, humectants, potting compounds, tire fill, inks, lubricants, antistatic agents, crude oil de-emulsifiers and plasticizers. As with any product, use of Arcol PPG-1000 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/cc
Bulk Density 62.5 lb/ft³
Viscosity 145 cP
Storage Temperature 15.0 - 60.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.020[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Flash Point 171 °CPMCC
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.030 %
 
Descriptive Properties
AppearanceClear, viscous liquid
Color<30 Pt-Co
Hydroxyl number107.4-115.4 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Arcol® F-3040 Polyol
Covestro Arcol® F-3022 Polyol
Covestro Arcol® LG-650 Polyether Polyol
Covestro Arcol® LHT-42 Polyether Polyol
Covestro Arcol® F-1522 Polyether Polyol

PCOVEST0033 / 201816

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.