MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Elkem Silicon 97
Categories: Metal; Nonferrous Metal

Material Notes: Silicon 97 is a large scale furnace produced and refined Silicon from Elkem. Unlike Silicon 98-99, it is a silicon grade containing typical 1,7% Fe, which gives a benefit in processes where Fe has to be added. Large furnace operation gives a high degree of consistency, both in analysis and in refining characteristics. The product has low calcium, slag and carbide content.

Silicon 97 is a refined grade silicon, containing max 0,05% Ca. The refining process guarantees a slag free product of high consistency. Silicon 97 dissolves easily and provides a high yield. Silicon 97 is an excellent silicon source for all aluminum alloys where iron is not a critical element. It can be used for all HP die-casting alloys, for hyper-eutectic alloys and for most AA 6000 extrusion billet alloys.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 10000 - 100000 µm10000 - 100000 µm
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.050 - 0.25 %0.050 - 0.25 %
Calcium, Ca 0.010 - 0.050 %0.010 - 0.050 %
Iron, Fe 1.5 - 2.0 %1.5 - 2.0 %
Phosphorus, P 0.0030 - 0.0055 %0.0030 - 0.0055 %
Silicon, Si 97 - 98 %97 - 98 %
Titanium, Ti 0.050 - 0.10 %0.050 - 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Alumor 4370 Thermal Ceramic
H.C. Starck Grade AX 20 Silicon Metal Powder Si
H.C. Starck Grade AX 10 Silicon Metal Powder Si

NELKEM10 / 16168

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.